Theoretical analysis of the alloying system and design of...

Theoretical analysis of the alloying system and design of new nickel-base superalloys

A. V. Logunov, I. M. Razumovskii, G. B. Stroganov, A. V. Ruban, V. I. Razumovskii, V. N. Larionov, O. G. Ospennikova, V. A. Poklad