![](/img/cover-not-exists.png)
Analytical Electron Microscopy Examination of the γ′/γ Interfaces in a Ni-Based Superalloy
K. Hodor, P. Zięba, B. Olszowska-SobierajVolume:
9
Language:
english
Pages:
6
DOI:
10.1023/a:1015106711353
Date:
November, 2001
File:
PDF, 1.17 MB
english, 2001