The role of hydrogen in the process of stress corrosion cracking of pipeline steels in dilute carbonate-bicarbonate solution
L. J. Qiao, J. L. Luo, X. MaoVolume:
16
Language:
english
Pages:
5
DOI:
10.1023/a:1018541116291
Date:
April, 1997
File:
PDF, 210 KB