Analysis of oxidation behavior of Ni-base superalloys by laser-induced breakdown spectroscopy
Kim, Tae-Hyeong, Lee, Dong-Hyoung, Kim, Donghoon, Jang, Changheui, Yun, Jong-IlVolume:
27
Year:
2012
Language:
english
Journal:
Journal of Analytical Atomic Spectrometry
DOI:
10.1039/c2ja30138e
File:
PDF, 1.37 MB
english, 2012