Fatigue strength and fatigue-fracture fractography of a chromium alloy of the Cr-V-B-Y system at temperatures of 20°C and 1100°C
V. F. Terent'ev, A. G. Fridman, Yu. K. Shtovba, G. V. Karsanov, S. V. Indenbaum, E. A. VoitekhovaVolume:
10
Language:
english
Pages:
4
DOI:
10.1007/bf01522319
Date:
December, 1978