An investigation on the creep and fracture behavior of cast nickel-base superalloy IN738LC
Guo Jianting, D. Ranucci, E. Picco, P. M. StrocchiVolume:
14
Language:
english
Pages:
7
DOI:
10.1007/bf02663308
Date:
November, 1983