Influence of molybdenum on the creep properties of nickel-base superalloy single crystals
R. A. MacKay, M. V. Nathal, D. D. PearsonVolume:
21
Language:
english
Pages:
8
DOI:
10.1007/bf02782418
Date:
January, 1990
File:
PDF, 1.60 MB
english, 1990