Anisotropic stress corrosion cracking behaviour of prestressing steel
J. Toribio, A. M. LanchaVolume:
49
Year:
1998
Language:
english
Pages:
5
DOI:
10.1002/(sici)1521-4176(199801)49:13.0.co;2-a