![](/img/cover-not-exists.png)
Study of the influence of welding parameters on the stress corrosion resistance of AISI 304 steel
C. V. Franco, R. P. Barbosa, A. E. Martinelli, A. J. A. BuschinelliVolume:
49
Year:
1998
Language:
english
Pages:
9
DOI:
10.1002/(sici)1521-4176(199807)49:73.0.co;2-2
File:
PDF, 333 KB
english, 1998