![](/img/cover-not-exists.png)
SEM observations on stress corrosion cracking of commercially pure titanium in a topical fluoride solution
Mauno H.O. Könönen, Eeva T. Lavonius, Jorma K. KivilahtiVolume:
11
Year:
1995
Language:
english
Pages:
4
DOI:
10.1016/0109-5641(95)80061-1
File:
PDF, 670 KB
english, 1995