Biochimica et Biophysica Acta (BBA) - Protein Structure and Molecular Enzymology
1984 Vol. 791; Iss. 2
![](/img/cover-not-exists.png)
A differential scanning calorimetry analysis of the age-related changes in the thermal stability of rat skin collagen
Fortuné Flandin, Chantal Buffevant, Daniel HerbageVolume:
791
Year:
1984
Language:
english
Pages:
7
DOI:
10.1016/0167-4838(84)90010-4
File:
PDF, 492 KB
english, 1984