![](/img/cover-not-exists.png)
The electrochemical characteristics of the galvanic corrosion of sulphide minerals in short-circuited model galvanic cells
Pawelł Nowak, Ewa Krauss, Andrzej PomianowskiVolume:
12
Year:
1984
Language:
english
Pages:
16
DOI:
10.1016/0304-386x(84)90050-1
File:
PDF, 918 KB
english, 1984