The hardness and strength of metal tribofilms: An apparent contradiction between nanoindentation and pillar compression
Corbett C. Battaile, Brad L. Boyce, Christopher R. Weinberger, Somuri V. Prasad, Joseph R. Michael, Blythe G. ClarkVolume:
60
Year:
2012
Language:
english
Pages:
9
DOI:
10.1016/j.actamat.2011.11.059
File:
PDF, 1.32 MB
english, 2012