Characterization of microshrinkage casting defects of Al–Si alloys by X-ray computed tomography and metallography
Gianni Nicoletto, Radomila Konečná, Stanislava FintovaVolume:
41
Year:
2012
Language:
english
Pages:
8
DOI:
10.1016/j.ijfatigue.2012.01.006
File:
PDF, 1.25 MB
english, 2012