![](/img/cover-not-exists.png)
Effect of boron addition on pitting corrosion resistance of modified 9Cr–1Mo steel: Application of electrochemical noise
M.G. Pujar, C.R. Das, S. Thirunavukkarasu, U. Kamachi Mudali, A.K. Bhaduri, J. Brijitta, B.V.R. TataVolume:
130
Year:
2011
Language:
english
Pages:
12
DOI:
10.1016/j.matchemphys.2011.07.036
File:
PDF, 2.74 MB
english, 2011