![](/img/cover-not-exists.png)
Deformation behavior during nanoindentation of epitaxial ZnO thin films on sapphire substrate
R. Navamathavan, Kyoung-Kook Kim, Dae-Kue Hwang, Seong-Ju Park, Tae Geol Lee, Gwang-Seok Kim, Jun-Hee HahnVolume:
61
Year:
2007
Language:
english
Pages:
3
DOI:
10.1016/j.matlet.2006.09.032
File:
PDF, 404 KB
english, 2007