![](/img/cover-not-exists.png)
Flow behavior and hot workability of FGH4096 superalloys with different initial microstructures by using advanced processing maps
Yongquan Ning, Zekun Yao, Zheng Yang, Hongzhen Guo, M.W. FuVolume:
531
Year:
2012
Language:
english
Pages:
7
DOI:
10.1016/j.msea.2011.10.039
File:
PDF, 1.92 MB