Suppressing the formation of SRZ in a Ni-based single crystal superalloy by RuNiAl diffusion barrier
Zhiming Bai, Dongqing Li, Hui Peng, Juan Wang, Hongbo Guo, Shengkai GongVolume:
22
Year:
2012
Language:
english
Pages:
7
DOI:
10.1016/j.pnsc.2012.03.007
File:
PDF, 1.07 MB
english, 2012