![](/img/cover-not-exists.png)
Effect of severe plastic deformation on grain boundary liquation of a nickel–base superalloy
S.M. Mousavizade, F. Malek Ghaini, M.J. Torkamany, J. Sabbaghzadeh, A. Abdollah-zadehVolume:
60
Year:
2009
Language:
english
Pages:
4
DOI:
10.1016/j.scriptamat.2008.10.021
File:
PDF, 273 KB
english, 2009