Strength estimation of different designs of ceramic inlays and onlays in molars based on the Tsai-Wu failure criterion
Beata Dejak, Andrzej Mlotkowski, Maciej RomanowiczVolume:
98
Year:
2007
Language:
english
Pages:
12
DOI:
10.1016/s0022-3913(07)60042-0