Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
2002 Vol. 191; Iss. 1-4
![](/img/cover-not-exists.png)
Nanoindentation mechanical properties characterization of glassy polymeric carbon treated with ion beam
M.G. Rodrigues, N.C. da Cruz, E.C. Rangel, R.L. Zimmerman, D. Ila, D.B. Poker, D.K. HensleyVolume:
191
Year:
2002
Language:
english
Pages:
6
DOI:
10.1016/s0168-583x(02)00604-3
File:
PDF, 123 KB
english, 2002