Analog-Circuit Model of FGH96 Superalloy Hot Deformation Behaviors Based on Artificial Neural Network
Yu-hong LIU, Fu-guo LI, Chao LI, Shi-chun WUVolume:
18
Year:
2005
Language:
english
Pages:
7
DOI:
10.1016/s1000-9361(11)60288-4
File:
PDF, 229 KB
english, 2005