Interaction between oxidation and thermo-mechanical fatigue in IN738LC superalloy — I
S. Esmaeili, C.C. Engler-Pinto Jr., B. Ilschner, F. Rézaï-AriaVolume:
32
Year:
1995
Language:
english
Pages:
1782
DOI:
10.1016/0956-716x(95)00004-f
File:
PDF, 385 KB
english, 1995