Hot corrosion behaviour of a cobalt-base super-alloy K40S...

Hot corrosion behaviour of a cobalt-base super-alloy K40S with and without NiCrAlYSi coating

K. Zhang, M.M. Liu, S.L. Liu, C. Sun, F.H. Wang