![](/img/cover-not-exists.png)
Hardness and Young's modulus of nanoporous EB-PVD YSZ coatings by nanoindentation
Byung-Koog Jang, Hideaki MatsubaraVolume:
402
Year:
2005
Language:
english
DOI:
10.1016/j.jallcom.2005.02.064
File:
PDF, 261 KB
english, 2005