Gamma prime coarsening and age-hardening behaviors in a new nickel base superalloy
Shuangqun Zhao, Xishan Xie, Gaylord D Smith, Shailesh J PatelVolume:
58
Year:
2004
Language:
english
DOI:
10.1016/j.matlet.2003.10.053