Effects of anisotropy on elastic moduli measured by nanoindentation in human tibial cortical bone
J. G. Swadener, Jae-Young Rho, G. M. PharrVolume:
57
Year:
2001
Language:
english
Pages:
5
DOI:
10.1002/1097-4636(200110)57:13.0.co;2-6
File:
PDF, 218 KB
english, 2001