SVET, AFM and AES study of pitting corrosion initiated on MnS inclusions by microinjection
B. Vuillemin, X. Philippe, R. Oltra, V. Vignal, L. Coudreuse, L.C. Dufour, E. FinotVolume:
45
Year:
2003
Language:
english
DOI:
10.1016/s0010-938x(02)00222-6
File:
PDF, 667 KB
english, 2003