![](/img/cover-not-exists.png)
Solidification process of conventional superalloy by confocal scanning laser microscope
Zhu-jun MIAO, Ai-dang SHAN, Wei WANG, Jun LU, Wen-liang XU, Hong-wei SONGVolume:
21
Year:
2011
Language:
english
DOI:
10.1016/s1003-6326(11)60704-8
File:
PDF, 1.22 MB
english, 2011