Effects of heat treatment and Re-content on the TCP-phase in two Ni-Mo-Cr-Re superalloys
Pingli MAO, Yan XIN, Ke HAN, Weiguo JIANGVolume:
22
Year:
2009
Language:
english
DOI:
10.1016/s1006-7191(08)60110-6
File:
PDF, 1.12 MB