Construction of a pseudo-binary phase diagram for multi-component Ni-base superalloys
Raghavan, S., Singh, Gaurav, Sondhi, Sanjay, Srikanth, S.Volume:
38
Language:
english
Journal:
Calphad
DOI:
10.1016/j.calphad.2012.04.003
Date:
September, 2012
File:
PDF, 1.33 MB