![](/img/cover-not-exists.png)
Electrochemical study of the pitting corrosion of aluminium and its alloys—III. The role of bonded water and the kinetics of formation and reformation of a passive layer
L. Tomcsányi, Zs. Nagy, J. Somlai, J. BorszékiVolume:
38
Year:
1993
Language:
english
Pages:
6
DOI:
10.1016/0013-4686(93)80150-x
File:
PDF, 516 KB
english, 1993