On the cyclic behavior of cast and extruded aluminum alloys. Part B: Fractography
R.J. Stofanak, R.W. Hertzberg, J. Leupp, R. JaccardVolume:
17
Year:
1983
Language:
english
Pages:
14
DOI:
10.1016/0013-7944(83)90114-5
File:
PDF, 2.40 MB
english, 1983