Initiation of stress corrosion cracking and fatigue crack under compressive stress
Chu Wu-Yang, Hsiao Chi-Mei, Liu Tian-Hua, Yao JingVolume:
20
Year:
1984
Language:
english
Pages:
9
DOI:
10.1016/0013-7944(84)90132-2
File:
PDF, 1.41 MB