![](/img/cover-not-exists.png)
Plasma deposition of ultrathin films of poly(2-hydroxyethyl methacrylate): surface analysis and protein adsorption measurements
Lopez, Gabriel P., Ratner, Buddy D., Rapoza, Richard J., Horbett, Thomas A.Volume:
26
Language:
english
Journal:
Macromolecules
DOI:
10.1021/ma00065a001
Date:
June, 1993
File:
PDF, 1.56 MB
english, 1993