A Novel Approach Based on Differential Scanning Calorimetry Applied to the Study of Tricalcium Silicate Hydration Kinetics †
Damasceni, Alessio, Dei, Luigi, Fratini, Emiliano, Ridi, Francesca, Chen, Sow-Hsin, Baglioni, PieroVolume:
106
Language:
english
Journal:
The Journal of Physical Chemistry B
DOI:
10.1021/jp020211l
Date:
November, 2002
File:
PDF, 175 KB
english, 2002