The effect of pitting corrosion on split sleeve cold hole expanded, bare 7075-T651 aluminium alloy
Stephen, Glenn J., Pasang, Timotius, Withy, Benjamin P.Volume:
15
Language:
english
Journal:
Journal of Manufacturing Processes
DOI:
10.1016/j.jmapro.2012.09.008
Date:
January, 2013