Effect of Varying Test Parameters on Elastic–plastic Properties Extracted by Nanoindentation Tests
L. Ladani, E. Harvey, S. F. Choudhury, C. R. TaylorVolume:
53
Language:
english
DOI:
10.1007/s11340-013-9732-7
Date:
October, 2013