Texture and surface analysis of NiO buffer deposited on biaxially textured Ni tapes by a MOCVD method
Jong-Won Sun,, Hyung Seop Kim,, Bong Ki Ji,, Hai-Woong Park,, Gye-Won Hong,, Choong-Hwan Jung,, Soon-Dong Park,, Byung-Hyuk Jun,, Chan-Joong Kim,Volume:
13
Language:
english
Journal:
IEEE Transactions on Appiled Superconductivity
DOI:
10.1109/TASC.2003.811842
Date:
June, 2003
File:
PDF, 727 KB
english, 2003