![](/img/cover-not-exists.png)
The effects of film thickness and incorporated anions on pitting corrosion of aluminum with barrier-type oxide films formed in neutral borate and phosphate electrolytes
Hiroki Habazaki, Rokuro Nishimura, Kenji Okitsu, Hiroyuki Inoue, Ikuo Kiriyama, Fumitaka Kataoka, Masatoshi Sakairi, Hideaki TakahashiVolume:
18
Language:
english
DOI:
10.1007/s10008-013-2192-2
Date:
February, 2014
File:
PDF, 490 KB
english, 2014