Superalloy 718 and Derivatives (Ott/Superalloy) || The Effect of Primary γ′ Distribution on Grain Growth Behavior of GH720Li Alloy
Ott, E.A., Groh, J.R., Banik, A., Dempster, I., Gabb, T.P., Helmink, R., Liu, X., Mitchell, A., Sjöberg, G.P., Wusatowska-Sarnek, A.Volume: