Susceptibility of highly alloyed austenitic stainless steels to caustic stress corrosion cracking
G. Rondelli, B. VicentiniVolume:
53
Year:
2002
Language:
english
Pages:
7
DOI:
10.1002/1521-4176(200211)53:113.0.co;2-d
File:
PDF, 1.07 MB
english, 2002