Characterization of deformation anisotropies in an α-Ti alloy by nanoindentation and electron microscopy
Kwon, J., Brandes, M.C., Sudharshan Phani, P., Pilchak, A.P., Gao, Y.F., George, E.P., Pharr, G.M., Mills, M.J.Volume:
61
Language:
english
Journal:
Acta Materialia
DOI:
10.1016/j.actamat.2013.05.005
Date:
August, 2013
File:
PDF, 4.95 MB
english, 2013