Inhomogeneous plastic deformation and its relevance to iodine stress corrosion cracking susceptibility in irradiated Zircaloy-2 Tubing
Takeo Onchi, Hideo Kayano, Yasuhiro HigashiguchiVolume:
116
Year:
1983
Language:
english
Pages:
8
DOI:
10.1016/0022-3115(83)90105-8
File:
PDF, 905 KB
english, 1983