A Microstructural and Fractographic Study on the Failure of Surgical Torch Meters
Barbosa, Cassio, Cerqueira Abud, Ibrahim, Barros, Tatiana Silva, Carvalho, Sheyla Santana, Caminha, Ieda Maria VieiraVolume: