Microstructural investigation of thermally aged nickel-based superalloy 718Plus
Whitmore, Lawrence, Ahmadi, Mohammad Reza, Stockinger, Martin, Povoden-Karadeniz, Erwin, Kozeschnik, Ernst, Leitner, HaraldVolume:
594
Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2013.11.037
Date:
January, 2014
File:
PDF, 1.76 MB
english, 2014