![](/img/cover-not-exists.png)
Galvanic corrosion of metal/ceramic coupling
Schneider, M., Kremmer, K., Lämmel, C., Sempf, K., Herrmann, M.Volume:
80
Language:
english
Journal:
Corrosion Science
DOI:
10.1016/j.corsci.2013.11.024
Date:
March, 2014
File:
PDF, 1.16 MB
english, 2014