![](/img/cover-not-exists.png)
Ceramic Femoral Component Fracture in Total Knee Arthroplasty: An Analysis Using Fractography, Fourier-Transform Infrared Microscopy, Contact Radiography and Histology
Krueger, Alexander P., Singh, Gurpal, Beil, Frank Timo, Feuerstein, Bernd, Ruether, Wolfgang, Lohmann, Christoph H.Volume:
29
Language:
english
Journal:
The Journal of Arthroplasty
DOI:
10.1016/j.arth.2013.11.003
Date:
May, 2014
File:
PDF, 513 KB
english, 2014