![](/img/cover-not-exists.png)
Flow curve determination of thin films by improved finite element models and different nanoindenter geometries
Bobzin, K., Bagcivan, N., Brugnara, R.H., Perne, J.Volume:
549
Language:
english
Journal:
Thin Solid Films
DOI:
10.1016/j.tsf.2013.06.037
Date:
December, 2013
File:
PDF, 1.11 MB