![](/img/cover-not-exists.png)
The corrosion fatigue fractography of Ti-24Al-11Nb
Zhang, Yue, Wang, Yue-Bin, Chu, Wu-Yang, Hsiao, Chi-MeiVolume:
30
Language:
english
Journal:
Scripta Metallurgica et Materialia
DOI:
10.1016/0956-716X(94)90426-X
Date:
March, 1994
File:
PDF, 477 KB
english, 1994